Synthesis Method Of Polyferric Sulfate

Polyferric sulfate liquid is produced by adding approximately 3% dilute sulfuric acid to ferrous sulfate, followed by the addition of sodium nitrite in a ratio of approximately 3:100. Oxidation is then initiated by introducing air or oxygen, followed by hydrolysis and polymerization to obtain polyferric sulfate.

 

The manufacturing method for solid polyferric sulfate is as follows: Using liquid ferrous sulfate as raw material, air is used as the oxidant. The process involves low-temperature dehydration, pulverization, high-temperature oxidation, cooling, polymerization, solidification, aging, and pulverization to obtain the final product.